Tensile properties and formability of low Ni (1.2 mass%Ni) metastable austenitic stainless steel sheets

Kanni Raj, A. ; Padmanabhan, K. A. (1998) Tensile properties and formability of low Ni (1.2 mass%Ni) metastable austenitic stainless steel sheets Materials Transactions, 39 (5). pp. 613-616. ISSN 1345-9678

Full text not available from this repository.

Official URL: http://www.jim.or.jp/journal/e/39/05/613.html

Abstract

Sheets of a low nickel (1.2 mass%Ni) metastable austenitic stainless steel, developed by some members of the Indian Stainless Steel Development Association, were tested for formability. The 0.70 mm thick sheets displayed inferior formability to the 0.90 mm thick sheets in all the three regions of forming-stretching, plane strain forming and deep drawing till a minor strain of -10%. This result was traced mainly to the lower sheet thickness and reduced straininduced martensite formation that leads to reduced work hardening. The forming limit diagrams predicted by a model due to Date and Padmanabhan correlated well with the experimental plots.

Item Type:Article
Source:Copyright of this article belongs to Japan Institute of Metals.
Keywords:Formability; Forming Limit Diagram; Low Nickel Stainless Steel; Metastable Austenitic Stainless Steel; Household Utensil Manufacture