Abrasion of Al2O3-SiC - (Al,Si) composites made by melt oxidation

Singh, R. Arvind ; Jayaram, Vikram ; Biswas, S. K. (1999) Abrasion of Al2O3-SiC - (Al,Si) composites made by melt oxidation Journal of Materials Research, 14 (1). pp. 64-67. ISSN 0884-2914

Full text not available from this repository.

Official URL: http://www.mrs.org/s_mrs/sec_subscribe.asp?CID=229...

Related URL: http://dx.doi.org/10.1557/JMR.1999.0011

Abstract

We report here the remarkable abrasion wear resistance (normal pressure: 2.92 to 5.42 MPa, sliding speed: 0.25 to 3 m/s) of a soft (relative to other structural ceramics) melt oxidized ceramic matrix composite Al203!=SiC!=(Al,Si). Inspite of being half as hard and more porous than zirconia toughened alumina (ZTA), a common cutting tool material, this composite fabricated at l l00 °C shows wear resistance comparable to that of ZTA at sliding speeds more than 2 m/s. The ability of this composite to generate a metal rich tribofilm when rubbed and its high thermal shock resistance are factors which may be responsible for this unique performance.

Item Type:Article
Source:Copyright of this article belongs to Materials Research Society.
ID Code:13629
Deposited On:12 Nov 2010 15:13
Last Modified:19 Feb 2011 04:56

Repository Staff Only: item control page